Introduction
When sourcing lined pipe fittings for abrasive slurry or wear-prone service, you will often see material datasheets citing ASTM G65 or ASTM G99 test results. These standards are valuable for ranking materials, but they are frequently misunderstood. This guide explains what each test measures, how to interpret the numbers, and what to verify before you rely on them for procurement decisions.
ASTM G65: Dry Sand/Rubber Wheel Abrasion Test
ASTM G65 measures resistance to scratching abrasion using a dry sand/rubber wheel apparatus. The test involves a rubber wheel pressing a specimen against a stream of dry sand. The result is reported as volume loss in cubic millimetres; lower volume loss means higher abrasion resistance.
The standard includes five procedures (A through E) that vary test severity and duration. Procedure A is a relatively severe test that ranks materials from low to extreme abrasion resistance. Procedure B is a short-term variation for medium- and low-abrasion-resistant materials. Procedure C is for thin coatings. Procedures D and E use lighter loads for specific applications.
According to the standard, the test is designed to produce data that reproducibly ranks materials in their resistance to scratching abrasion under a specified set of conditions. It does not attempt to duplicate all process conditions such as abrasive size, shape, pressure, impact, or corrosive elements. Therefore, it should not be used to predict exact resistance in a specific environment. Its value lies in predicting the relative ranking of materials in a similar order of merit as would occur in an abrasive environment.