Why SCC Testing Needs Two Distinct Decisions
Stress-corrosion cracking (SCC) is not a single test. For chloride SCC screening of stainless steels and related alloys, ASTM G36 provides the exposure environment: boiling magnesium chloride solution held at 155.0 °C ± 1.0 °C (311.0 °F ± 1.8 °F) at one atmosphere pressure. ASTM G30 provides one specimen configuration: the U-bend. The two documents work together, but they address separate variables. As a buyer, you must specify both the environment and the loading configuration to get a defensible test plan.
What ASTM G36 Covers
ASTM G36 is a Standard Practice for Evaluating Stress-Corrosion-Cracking Resistance of Metals and Alloys in a Boiling Magnesium Chloride Solution. It is an accelerated method for ranking the relative degree of SCC susceptibility for stainless steels and related alloys in aqueous chloride-containing environments. The practice is applicable to wrought, cast, and welded stainless steels and related alloys. It can detect the effects of composition, heat treatment, surface finish, microstructure, and stress on susceptibility to chloride SCC.
The practice is concerned primarily with the test solution. It may be used with a variety of SCC test specimens, surface finishes, and methods of applying stress. The standard also describes a suggested test apparatus capable of maintaining solution concentration and temperature within prescribed limits for extended periods.
Important cautions from the standard: